Hardfacing Basics: Rebuilding Worn Parts with Welding

10.10.26 05:37 PM By Varun Menon

Welder Tips5 min readMentrode Welding Electrodes

How hardfacing electrodes extend the life of crusher hammers, bucket teeth and rollers – and how to pick the right hardness.

Parts that wear – crusher hammers, excavator bucket teeth, sugar mill rollers, conveyor screws, shafts – don't always need replacing. Hardfacing adds a hard, wear-resistant layer by welding, often lasting longer than the original part.

Know the type of wear

WearExample partsTypical choice
Metal-to-metal (rolling, sliding)Shafts, rollers, wheels, gear teethLower hardness, about 30–35 HRC, machinable
Impact with some abrasionCrusher hammers, rail crossingsMedium hardness about 48 HRC, or 14% manganese for heavy impact
Severe abrasionBucket teeth, mixer blades, screw conveyorsHigh hardness, about 60–64 HRC or chromium-carbide

HRC = Rockwell C hardness. Higher numbers resist abrasion better but are more brittle and usually can't be machined.

Build-up then hardface

If a part is badly worn, first rebuild it close to size with a tough build-up electrode, then finish with one or two layers of hardfacing. Too many hard layers can crack and spall off.

Good practice

  • Clean off rust, oil and old cracked hardfacing.
  • Preheat thick or high-carbon parts (often 150–250 °C) to avoid cracking.
  • Use stringer beads or a light weave, overlapping each bead by about a third.
  • Small cross-cracks (check cracks) in very hard deposits are normal and relieve stress.
  • Let the part cool slowly.
Hardfacing electrodes in 30, 35, 48 and 64 HRC, plus graphite-type, are available from us made to order. Tell us the part and the type of wear and we'll recommend a grade.

Varun Menon

Items have been added to cart.
One or more items could not be added to cart due to certain restrictions.
Added to cart
Quantity updated
- An error occurred. Please try again later.
Deleted from cart
- Can't delete this product from the cart at the moment. Please try again later.