How to recognise the most common stick welding defects, what causes them and the simple changes that fix them.
Most weld defects come from a handful of causes – wrong current, wrong arc length, damp electrodes or a dirty joint. Learn to read the weld and the fix is usually quick.
Porosity (pin holes)
Small holes on the surface or inside the weld, caused by gas trapped as the metal freezes.
- Causes: damp electrodes, rust/oil/paint on the joint, long arc, wind blowing the shielding away, current too high on low-hydrogen rods.
- Fixes: dry or re-dry electrodes, clean the joint to bright metal, hold a short arc, screen the work from wind.
Cracks
The most serious defect – a crack can grow and cause the joint to fail.
- Hot cracks (centre of the bead as it cools): deep narrow beads, high sulphur in the steel, a concave crater at the end. Fix: wider, flatter beads and fill the crater before breaking the arc.
- Cold or hydrogen cracks (hours after welding, next to the weld): hydrogen from damp electrodes plus hard, thick or restrained steel. Fix: use dry low-hydrogen electrodes (E7016/E7018), preheat thick plate, avoid fast cooling.
Undercut
A groove melted into the plate along the edge of the weld that is not filled. It weakens the joint.
- Causes: current too high, travelling too fast, wrong electrode angle, long arc.
- Fixes: reduce current, slow down, pause briefly at the edges when weaving.
Slag inclusions
Slag trapped between passes. Fix: chip and brush every pass clean, raise the current slightly, avoid deep narrow grooves.
Lack of fusion and penetration
Weld metal sitting on the plate without melting into it. Fix: more current, correct joint gap and bevel, the right electrode angle and a smaller electrode for the root.
Excess spatter
Fix: lower the current, shorten the arc, use dry electrodes and check polarity.