Welding Current Chart by Electrode Size – and Why Amperage Matters

10.10.26 03:58 PM By Varun Menon

Welder Tips6 min readMentrode Welding Electrodes

The right amperage for every electrode size, what happens when it is too high or too low, and how adjusting it gives you better welds.

Current is the one setting every welder changes – and the one most often set wrong. Get it right and the arc is smooth, the bead is neat and the slag lifts off. Get it wrong and you fight the electrode all day.

Current chart for Mentrode electrodes

SizeE6013E7016E7018
2.5 / 2.6 mm60 – 90 A60 – 90 A70 – 110 A
3.15 / 3.2 mm90 – 130 A90 – 130 A90 – 140 A
4.0 mm130 – 170 A130 – 180 A140 – 190 A
5.0 mm170 – 220 A180 – 240 A190 – 250 A

A handy rule of thumb: about 35–40 amps per millimetre of electrode diameter. For vertical and overhead welding, use 10–15% less current. Try our current calculator.

Why amperage matters

Current controls how much heat goes into the joint. Heat decides how deep the weld goes (penetration), how fast the electrode melts and how the weld pool behaves.

Current too low

  • Electrode sticks to the job
  • Hard to strike and keep the arc
  • Narrow, humped bead sitting on top
  • Poor penetration and lack of fusion
  • Slag trapped in the weld

Current too high

  • Electrode glows red and the coating cracks
  • Lots of spatter
  • Undercut along the edges
  • Burn-through on thin metal
  • Porosity, especially with low-hydrogen electrodes

The benefits of adjusting it properly

  • Stronger joints – correct penetration fuses the weld into both plates.
  • Less grinding and rework – less spatter, less undercut, easy slag removal.
  • Less wasted electrode – no stubs thrown away after sticking, no overheated half-used rods.
  • Faster work – the right current gives a steady travel speed and a bead that needs no repair.
  • Fewer hidden defects – most porosity, slag inclusion and lack-of-fusion problems start with the wrong current.

How to set it

  1. Start in the middle of the range for your size.
  2. Run a short bead on scrap of the same thickness.
  3. Sticking or a humped bead? Go up 5–10 A. Spatter, undercut or a red-hot electrode? Go down 5–10 A.
  4. Adjust again for position – a little lower for vertical-up and overhead.
Note: the dial on many machines is not exact. Use the bead and the sound – a steady, crisp crackle – as your guide.

Varun Menon

Items have been added to cart.
One or more items could not be added to cart due to certain restrictions.
Added to cart
Quantity updated
- An error occurred. Please try again later.
Deleted from cart
- Can't delete this product from the cart at the moment. Please try again later.